Note: Preheating for forging of steel pins

Objective:

To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.

End Product:

Wheel rim spokes

Equipment:

To heat magnetic steel pins (spokes) for forging on a rim without heat treating and weakening the rim. Previously, a torch was utilized and the heating time was 20 seconds.

Materials:

9/16 in  (14 mm) steel pins

Temperature:

2,000 °F (1,093 °C)

Frequency:

294 kHz

Testing:

A single=position three-turn helical coil was used, and the part was placed under the coil. The part was heated to the desired temperature within just seven seconds.

Benefits:

  • Fast, precise heating of the pin‚Ă‚Â‚Ä‚Â‹Ă‚Â˜Ă„Â‚Ă‚Â‚Ä‚Â‚Ă‚Â€Ă„Â‚Ă‚Â‚Ä‚Â‚Ă‚Â“ 2 minutes and 36 seconds were saved on heating all of the rim"s pins when compared to using a torch.

  • The rim was not heated, which maintained its strength and durability.

  • Energy was saved due to the reduction in heating time.

  • There is more repeatability with induction when compared to using a torch.