In this note...
A fourteen-turn coil is used to heat 3.9” (100mm) of zinc wire for this zinc wire application. The wire is placed in the coil for 5 seconds to reach the desired condition just prior to the forming process.
Get your Free annealing Application Note
'Annealing a zinc wire prior to forming pellets for air rifles'
See how we've applied our remarkable induction heating solutions to solve our clients' annealing challenges.