In this note...
A three-turn helical coil is used to anneal the steel hydraulic motor shaft. The end of the motor shaft is placed in the coil and power is applied for 20 seconds to reach 1350 °F (732 °C) and turn the steel red hot before machining.
Get your Free annealing Application Note
'Annealing the end of a hydraulic motor shaft prior to machining'
See how we've applied our remarkable induction heating solutions to solve our clients' annealing challenges.